Simultaneous degradation by corrosion and wear of titanium in artificial saliva containing fluorides

dc.contributor.authorSouza, J. C. M.
dc.contributor.authorBarbosa, S. L.
dc.contributor.authorAriza, E.
dc.contributor.authorCelis, J. P.
dc.contributor.authorRocha, L. A.
dc.date.accessioned2012-07-06T16:19:03Z
dc.date.available2012-07-06T16:19:03Z
dc.date.issued2012
dc.date.submitted2012
dc.description.abstracthe degradation of titanium-based oral rehabilitation systems can occur by corrosion and wear processes taking place simultaneously (tribocorrosion) and influenced by the presence of fluorides. In this study, the tribocorrosion behavior of titanium in artificial saliva solutions containing fluorides is investigated. Before sliding tests were started up, electrochemical measurements such as open circuit potential (OCP) and impedance spectroscopy (EIS) were performed to get information on the corrosion behavior of titanium in artificial saliva solutions. Then, sliding wear tests were carried out at the OCP taken by the test sample. Scanning electron microscopy and weight loss measurements were performed after the tribocorrosion tests. The presence of a compact passive surface film on titanium immersed was demonstrated in artificial saliva free of fluorides and in presence of up to 227 ppm F−. However, a progressive degradation of titanium was observed at a F− concentration of 12,300 ppm. Additionally, the corrosion and wear resistance of the titanium oxide film formed at a F− concentration of 12,300 ppm differ from the ones obtained up to 227 ppm F− reflected by a decrease of the coefficient of friction although the material loss increased. The synergism between wear and corrosion processes on titanium needs thus to be further investigated to reach a reliable prediction of the long-term behavior of titanium-based prostheses and implants in the oral cavity.por
dc.description.sponsorshipFlemish Science Foundation - WOG-FWO-Vlaanderenpor
dc.description.sponsorshipAlBan Program - cod. E06D103407BR), e Flemish Science Foundation (WOG-FWO-Vlaanderen).por
dc.description.sponsorshipScientific research Community on Surface Modification of Materialspor
dc.description.sponsorshipFundação para a Ciência e a Tecnologia (FCT) - PTDC/CTM/67500/2006por
dc.distributioninternationalpor
dc.identifier.doi10.1016/j.wear.2012.05.030por
dc.identifier.issn0043-1648por
dc.identifier.urihttps://hdl.handle.net/1822/19840
dc.language.isoengpor
dc.peerreviewedyespor
dc.publisherElsevierpor
dc.relation.publisherversionhttp://www.sciencedirect.com/science/article/pii/S0043164812002050por
dc.rightsrestrictedAccesspor
dc.subjectTitaniumpor
dc.subjectCorrosionpor
dc.subjectDegradationpor
dc.subjectFluoridespor
dc.subjectTribocorrosionpor
dc.subjectWearpor
dc.subject.wosScience & Technologypor
dc.titleSimultaneous degradation by corrosion and wear of titanium in artificial saliva containing fluoridespor
dc.typearticlepor
dspace.entity.typePublicationen
oaire.citationEndPage88por
oaire.citationStartPage82por
oaire.citationTitleWearpor
oaire.citationVolume292por
sdum.journalWearpor
sdum.publicationstatusin publicationpor

Ficheiros

Pacote original

A mostrar 1 - 1 de 1
A carregar...
Nome:
Souza_Corrosion and wear of titanium in fluorides.pdf
Tamanho:
979.85 KB
Formato:
Adobe Portable Document Format